MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Butyrate, Molded

Material Notes: Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.

Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. TENITE cellulosic plastics are available in natural, clear, selected ambers, or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. TENITE Cellulose Acetate Butyrate 264-10 has a plasticizer level of 10%. It meets FDA requirements when supplied in FDA color numbers.

Applications: Toys/Sporting goods

Formula 264 - base; Meets FDA requirements when supplied in FDA color numbers.

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given

Information provided by Eastman Chemical.

Key Words: CAB
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Water Absorption 1.4 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 78ASTM D785
Tensile Strength, Ultimate 43.4 MPaASTM D638
Tensile Strength, Yield 33.1 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Yield Strength 45.5 MPaASTM D790
Flexural Modulus 1.379 GPaASTM D790
Izod Impact, Notched 2.40 J/cmASTM D256
 0.960 J/cm
@Temperature -40.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.55
@Frequency 1e+6 Hz
ASTM D 150
Dielectric Strength 15.25 kV/mmASTM D149
Dissipation Factor 0.080
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 17.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.465 J/g-°CDSC
Thermal Conductivity 0.250 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CConditioned 4 hours @ 70°C (158°F); ASTM D648
Vicat Softening Point 104 °CConditioned 4 hours @ 70°C (158°F); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.475ASTM D542
Haze <= 8.5 %
@Thickness 1.52 mm
ASTM D1003
Transmission, Visible >= 90 %
@Thickness 1.52 mm
ASTM E308

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP PPC 0412 R Blk Reprocessed Polypropylene, Unfilled
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene
Calcium Boride, CaB6
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate

PEA100 / 35234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.