MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman Eastar™ Renew DN501-10 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Eastar™ Renew DN501-10 copolyester is a high flow product designed and engineered for many different applications. With its excellent color and clarity and its ability to mold thick parts with improved gate aesthetics, Eastar™ Renew DN501-10 is clearly a well-suited copolyester for many applications. Other outstanding features are excellent chemical resistance, high gloss, and improvements in processing such as faster cycle times, and lower scrap rates. Eastar™ Renew DN501-10 is also ideally suited for two-shot molding due to its lower processing temperatures, very slow crystallization rate, and flow characteristics. Eastar™ Renew DN501-10 contains a mold release derived from vegetable based sources. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Electronics
Key Attributes
  • Ability to mold thick parts
  • Ease of processing
  • Easy to extrude, cut, decorate, and seal
  • Excellent clarity and color
  • Excellent colorability
  • Good chemical resistance
  • Good impact strength
  • Good stiffness
  • High gloss appearance
  • Improved gate aesthetics
  • Readily fill intricate molds
  • Toughness

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.00450 cm/cm0.00450 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102.1102.1ASTM D785
Tensile Strength at Break 28.2 MPa4090 psiISO 527
 50.5 MPa7320 psiASTM D638
Tensile Strength, Yield 45.0 MPa6530 psiISO 527
 48.0 MPa6960 psiASTM D638
Elongation at Break 201.7 %201.7 %ISO 527
 350.4 %350.4 %ASTM D638
Elongation at Yield 4.50 %4.50 %ASTM D638
 4.90 %4.90 %ISO 527
Tensile Modulus 1.6396 GPa237.80 ksiASTM D638
Flexural Yield Strength 68.94 MPa9999 psiASTM D790
Flexural Modulus 1.9314 GPa280.13 ksiASTM D790
Izod Impact, Notched  0.609 J/cm
@Temperature -40.0 °C
1.14 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 9.20 J/cm
@Temperature 23.0 °C
17.2 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  28.403 J/cm
@Temperature 23.0 °C
53.210 ft-lb/in
@Temperature 73.4 °F
ASTM D4812
 31.685 J/cm
@Temperature -40.0 °C
59.359 ft-lb/in
@Temperature -40.0 °F
ASTM D4812
Puncture Energy  48.9 J
@Temperature -40.0 °C
36.1 ft-lb
@Temperature -40.0 °F
@ Max. Load; ASTM D3763
 63.2 J
@Temperature 23.0 °C
46.6 ft-lb
@Temperature 73.4 °F
@ Max. Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.9 °C160 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.1 °C146 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.550 %0.550 %ASTM D1003
Transmission, Visible 90.8 %90.8 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 - 240 °C424 - 464 °F
Mold Temperature 16.0 - 38.0 °C60.8 - 100 °F
Drying Temperature 65.0 - 70.0 °C149 - 158 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4123 / 323746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.