MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acetal Copolymer, Unreinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.950 - 1.71 g/ccAverage value: 1.41 g/cc Grade Count:596
Water Absorption 0.0500 - 4.00 %Average value: 0.412 % Grade Count:214
 0.330 - 0.330 %
@Temperature 50.0 - 50.0 °C
Average value: 0.330 % Grade Count:3
 0.330 - 0.330 %
@Time 86400 - 86400 sec
Average value: 0.330 % Grade Count:3
Moisture Absorption at Equilibrium 0.0200 - 2.30 %Average value: 0.264 % Grade Count:157
Water Absorption at Saturation 0.220 - 8.00 %Average value: 0.883 % Grade Count:95
Maximum Moisture Content 0.0200 - 0.150Average value: 0.112 Grade Count:39
 0.200 - 0.300
@Temperature 100 - 100 °C
Average value: 0.250 Grade Count:2
 0.200 - 0.300
@Time 299 - 299 sec
Average value: 0.250 Grade Count:2
Linear Mold Shrinkage 0.00210 - 0.0360 cm/cmAverage value: 0.0204 cm/cm Grade Count:392
 0.0200 - 0.0220 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.0207 cm/cm Grade Count:8
Linear Mold Shrinkage, Transverse 0.00210 - 0.0335 cm/cmAverage value: 0.0201 cm/cm Grade Count:162
 0.0180 - 0.0190 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.0185 cm/cm Grade Count:8
Melt Flow 0.200 - 58.8 g/10 minAverage value: 14.3 g/10 min Grade Count:454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 52.4 - 86.2Average value: 61.5 Grade Count:4
Hardness, Rockwell M 30.0 - 97.0Average value: 79.3 Grade Count:153
Hardness, Rockwell R 69.0 - 130Average value: 104 Grade Count:72
Hardness, Shore D 70.0 - 86.0Average value: 80.4 Grade Count:28
Ball Indentation Hardness 30.0 - 180 MPaAverage value: 137 MPa Grade Count:85
Tensile Strength, Ultimate 6.37 - 71.0 MPaAverage value: 56.5 MPa Grade Count:268
 28.0 - 68.0 MPa
@Temperature -40.0 - 80.0 °C
Average value: 42.1 MPa Grade Count:3
Tensile Strength, Yield 21.0 - 75.8 MPaAverage value: 59.8 MPa Grade Count:368
 25.0 - 94.4582 MPa
@Temperature -40.0 - 120 °C
Average value: 55.5 MPa Grade Count:5
Elongation at Break 1.50 - 250 %Average value: 35.0 % Grade Count:519
 15.0 - 98.0 %
@Temperature -40.0 - 90.0 °C
Average value: 84.0 % Grade Count:10
Elongation at Yield 6.50 - 50.0 %Average value: 11.5 % Grade Count:202
 5.80 - 10.0 %
@Temperature -40.0 - 80.0 °C
Average value: 8.37 % Grade Count:2
Modulus of Elasticity 0.586 - 11.7 GPaAverage value: 2.66 GPa Grade Count:376
 0.480 - 4.50 GPa
@Temperature -40.0 - 90.0 °C
Average value: 1.71 GPa Grade Count:10
 2.41 - 2.81 GPa
@Temperature 30.0 - 120 °C
Average value: 1.71 GPa Grade Count:1
 2.41 - 2.81 GPa
@Thickness 1.50 - 4.00 mm
Average value: 1.71 GPa Grade Count:1
Flexural Yield Strength 24.0 - 862 MPaAverage value: 83.5 MPa Grade Count:371
Flexural Modulus 0.00144 - 7.38 GPaAverage value: 2.46 GPa Grade Count:436
Compressive Yield Strength 8.27 - 110 MPaAverage value: 50.1 MPa Grade Count:36
Compressive Modulus 1.03 - 2.76 GPaAverage value: 2.15 GPa Grade Count:17
Poissons Ratio 0.350 - 0.430Average value: 0.363 Grade Count:6
Fatigue Strength 22.8 - 31.0 MPaAverage value: 27.1 MPa Grade Count:4
Shear Strength 40.0 - 55.2 MPaAverage value: 52.2 MPa Grade Count:20
Izod Impact, Notched 0.320 J/cm - NBAverage value: 1.16 J/cm Grade Count:185
 0.300 - 1.00 J/cm
@Temperature -40.0 - -29.0 °C
Average value: 0.569 J/cm Grade Count:11
Izod Impact, Unnotched 0.363 J/cm - NBAverage value: 5.36 J/cm Grade Count:28
Izod Impact, Notched (ISO) 2.50 - 19.8 kJ/m²Average value: 7.26 kJ/m² Grade Count:113
 3.99 - 7.00 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 5.61 kJ/m² Grade Count:30
Izod Impact, Unnotched (ISO) 100 kJ/m² - NBAverage value: 407 kJ/m² Grade Count:10
 100 - 100 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 100 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.40 J/cm² - NBAverage value: 17.9 J/cm² Grade Count:157
 2.00 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 18.7 J/cm² Grade Count:89
Charpy Impact, Notched 0.140 J/cm² - NBAverage value: 0.703 J/cm² Grade Count:364
 0.250 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 0.605 J/cm² Grade Count:90
 1.30 - 1.30 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.605 J/cm² Grade Count:1
 1.30 - 1.30 J/cm²
@Thickness 4.00 - 4.00 mm
Average value: 0.605 J/cm² Grade Count:1
Gardner Impact 22.6 - 60.0 JAverage value: 33.5 J Grade Count:8
Tensile Impact Strength 5.78 - 1060 kJ/m²Average value: 240 kJ/m² Grade Count:8
Falling Dart Impact 22.6 - 32.1 JAverage value: 27.8 J Grade Count:3
Instrumented Impact Total Energy 16.5 - 18.4 JAverage value: 17.2 J Grade Count:3
Coefficient of Friction 0.0980 - 0.800Average value: 0.294 Grade Count:96
Coefficient of Friction, Static 0.110 - 0.330Average value: 0.157 Grade Count:24
Tensile Creep Modulus, 1 hour 1800 - 2500 MPaAverage value: 2270 MPa Grade Count:15
Tensile Creep Modulus, 1000 hours 400 - 1450 MPaAverage value: 1210 MPa Grade Count:57
K (wear) Factor 0.200 - 10000 x 10-8 mm³/N-MAverage value: 793 x 10-8 mm³/N-M Grade Count:53
Limiting Pressure Velocity 0.100 - 0.600 MPa-m/secAverage value: 0.360 MPa-m/sec Grade Count:4
Taber Abrasion, mg/1000 Cycles 14.0 - 350Average value: 55.3 Grade Count:21
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.200 - 1.00e+16 ohm-cmAverage value: 1.74e+15 ohm-cm Grade Count:300
Surface Resistance 100 - 3.00e+16 ohmAverage value: 3.84e+15 ohm Grade Count:313
Static Decay 0.00300 - 2.00 secAverage value: 1.34 sec Grade Count:6
Dielectric Constant 3.40 - 5.00Average value: 3.83 Grade Count:157
Dielectric Strength 15.7 - 86.6 kV/mmAverage value: 26.2 kV/mm Grade Count:206
Dissipation Factor 0.00100 - 0.530Average value: 0.0106 Grade Count:134
Dielectric Loss Index 0.00200 - 0.00800Average value: 0.00418 Grade Count:8
Arc Resistance 1.90 - 240 secAverage value: 121 sec Grade Count:23
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:114
Hot Wire Ignition, HWI 0.000 - 15.0 secAverage value: 9.13 sec Grade Count:4
High Amp Arc Ignition, HAI 120 arcsAverage value: 120 arcs Grade Count:4
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 216 µm/m-°CAverage value: 109 µm/m-°C Grade Count:320
CTE, linear, Transverse to Flow 20.0 - 180 µm/m-°CAverage value: 116 µm/m-°C Grade Count:112
Specific Heat Capacity 1.30 - 1.50 J/g-°CAverage value: 1.46 J/g-°C Grade Count:26
Thermal Conductivity 0.231 - 0.390 W/m-KAverage value: 0.304 W/m-K Grade Count:36
Melting Point 160 - 186 °CAverage value: 167 °C Grade Count:349
Maximum Service Temperature, Air 47.0 - 150 °CAverage value: 108 °C Grade Count:128
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 316 °CAverage value: 156 °C Grade Count:207
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 205 °CAverage value: 101 °C Grade Count:537
Vicat Softening Point 71.7 - 180 °CAverage value: 149 °C Grade Count:127
Heat Distortion Temperature 72.2 - 98.0 °CAverage value: 84.0 °C Grade Count:5
Minimum Service Temperature, Air -50.0 - -20.0 °CAverage value: -40.7 °C Grade Count:29
Glass Transition Temp, Tg -65.0 - -50.0 °CAverage value: -58.4 °C Grade Count:16
Decomposition Temperature 240 °CAverage value: 240 °C Grade Count:21
UL RTI, Electrical 50.0 - 110 °CAverage value: 104 °C Grade Count:7
UL RTI, Mechanical with Impact 50.0 - 95.0 °CAverage value: 87.1 °C Grade Count:6
UL RTI, Mechanical without Impact 50.0 - 100 °CAverage value: 91.7 °C Grade Count:6
Flammability, UL94 HB - V-2Grade Count:335
Oxygen Index 15.0 - 18.0 %Average value: 15.8 % Grade Count:4
Ignition Temperature 320 - 340 °CAverage value: 330 °C Grade Count:22
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 300 °CAverage value: 197 °C Grade Count:81
Nozzle Temperature 170 - 227 °CAverage value: 194 °C Grade Count:61
Melt Temperature 100 - 230 °CAverage value: 194 °C Grade Count:229
Mold Temperature 40.0 - 140 °CAverage value: 82.7 °C Grade Count:264
Injection Velocity 20.0 - 90.0 mm/secAverage value: 41.1 mm/sec Grade Count:9
Drying Temperature 71.1 - 121 °CAverage value: 91.9 °C Grade Count:211
Moisture Content 0.0200 - 0.200 %Average value: 0.110 % Grade Count:43
Dew Point -31.7 °CAverage value: -31.7 °C Grade Count:3
Injection Pressure 2.76 - 118 MPaAverage value: 52.7 MPa Grade Count:73
Vent Depth 0.00127 cmAverage value: 0.00127 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Homopolymer, Unreinforced
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced

O1250 / 77839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.