MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary Evoprene™ G 3292 SEBS Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxidation, ozone and general outdoor weathering is excellent.
Processing: compatible with polypropylene for co-molding or co-extrusion
Can be used in food contact applications with the appropriate stabilizer package

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/ccISO 2782
Viscosity Measurement 16
@Temperature 180 °C
Kg/cm2; Macklow-Smith extrusion rheometer
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37ISO 868
Tensile Strength 6.10 MPaISO 37
Elongation at Break 620 %ISO 37
100% Modulus 0.000800 GPa
@Strain 100 %
ISO 37
Tear Strength 18.0 kN/mISO 34-B
Compression Set 39 %
@Temperature 22.0 °C,
Time 259000 sec
ISO 815
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cm
Dielectric Strength 24.0 - 28.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 - 120 °C
Minimum Service Temperature, Air -60.0 - -40.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not specified
 
Descriptive Properties
Bonds withPolypropylene
Chemical ResistanceAcetoneModerate/Good
 Acids up to 80%Excellent
 AlcoholExcellent
 AlkalisExcellent
 Brake fluidGood
 Chlorinate solventsPoor
 DieselPoor
 Ethylene glycolExcellent
 GasolinePoor
 Salt solutionExcellent
 Soda lyeExcellent
 Water, 23°CExcellent
 Water, 95°CGood
TransparencyTransparent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ G 3315 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 3291 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ COGEE 631 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ COGEE 637 SEBS Thermoplastic Elastomer

PGARY9672 / 140465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.