MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® BM 20 SBG PA*
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grilon BM 20 SBG is a lactam free multipolyamide. Grilon BM 20 SBG has the following features:
  • Lactam free
  • Good transparency and gloss
  • Good flexibility and toughness
  • Very good thermoforming and shrink properties
Application: Grilon BM 20 SBG is suitable for the production of coextruded blown and cast films. Grilon BM 20 SBG is suitable for the following applications: Flexible packaging for foodstuffs and especially suitable for medical packaging applications such as intravenous bags.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccDry; ISO 1183
Water Absorption 6.0 %Sim. to ISO 62
Moisture Absorption 2.50 %Sim. to ISO 62
Water Vapor Transmission 20.0 g/m²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 40 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 30.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPaISO 527-3
Film Elongation at Break, MD 900 %ISO 527-3
Film Elongation at Break, TD 900 %ISO 527-3
Film Elongation at Yield, MD 10 %ISO 527-3
Film Elongation at Yield, TD 10 %ISO 527-3
Tensile Modulus 650 MPaConditioned; ISO 527-1/-2
Tear Strength 50.0 kN/mTrouser Tear Resistance, Parallel; ISO 6383-1
 75.0 kN/mTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 70.0 MPaISO 527-3
Film Tensile Strength at Break, TD 60.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °C10°C/min; ISO 11357-1/-3
 
Optical PropertiesOriginal ValueComments
Gloss 130 %60°; ISO 2813
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)250ISO 15105-1/-2; 23°C/ 85% RH
 80ISO 15105-1/-2; 23°C/0% RH
Elmendorf Tear Resistance, Normal (N)20ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)20ISO 6383-2
EMS Gelboflextest [holes/m²]200
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS200
Oxygen Transmission Rate, cm³/(m²*d*bar)25ISO 15105-1/-2; 23°C/0% RH
 70ISO 15105-1/-2; 23°C/ 85% RH
PackagingNon oriented film
 Oriented film
 Paper coating
ProcessingBlown Film Extrusion
 Film Extrusion
 Other Extrusion
Product AttributesBarrier Properties
 Co Polyamide
 High viscosity
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 12
DuPont Mobility and Materials Zytel® 42A NC010 PA66

PGRH203 / 156912

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.