MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® CP-18152 CLR Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-18152 CLR is a high performance thermoplastic elastomer designed for a variety of industrial and consumer product applications requiring a soft, rubber-like feel. Monprene CP-18152 CLR is a low density, low hardness, RoHS compliant grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: General Purpose; Good Adhesion; Good Colorability; Good Moldability; Good Tear Strength; Good Tensile Strength; High Clarity; High Elongation; High Flow; High Toughness; Low Density; Low Specific Gravity; Slip; Low Hardness; Without Fillers

Uses: Consumer Applications; Flexible Grip; General Purpose; Industrial Applications; Rubber Replacement; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 56
@Time 5.00 sec
ASTM D2240
 58
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 2000 psi20 in/min, Flow; ASTM D412
Tensile Stress at Strain 480 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 600 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 800 %20 in/min, Flow; ASTM D412
Tear Strength 235 pli20 in/min, Flow; ASTM D624
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 320 °F
Middle Barrel Temperature 340 - 380 °F
Front Barrel Temperature 380 - 410 °F
Nozzle Temperature 410 - 440 °F
Melt Temperature 380 - 440 °F
Mold Temperature 95.0 - 120 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0792 / 237283

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.