MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Niagara LaSalle 8620 Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel

Material Notes: The most widely used carburizing alloy. Its nickel content imparts good toughness and ductility. The chromium and molybdenum increases hardness penetration and wearability. This steel's well balanced alloy content permits hardening to produce a strong, tough core and high case hardness. It machines at 110 sfm and has good welding qualities.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.18 - 0.23 %
Chromium, Cr 0.40 - 0.60 %
Iron, Fe 96.895 - 98.02 %as balance
Manganese, Mn 0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8620 Steel, quenched from carburizing box, 50 mm (2 in.) round
AISI 8620 Steel, annealed 13 mm (0.5 in.) round
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
AISI 8620 Steel, normalized, 13 mm (0.5 in.) round
Niagara LaSalle 1213 Cold Finished Steel Bar

NNIAL015 / 160305

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.