MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Magnesium PE, Photoengraving Grade
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Key Words: Mg
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000100 ohm-cm0.0000100 ohm-cmEstimated from trends in similar alloys.
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 340 J/g146 BTU/lb
CTE, linear  26.0 µm/m-°C
@Temperature 0.000 - 100 °C
14.4 µin/in-°F
@Temperature 32.0 - 212 °F
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
Specific Heat Capacity 1.047 J/g-°C0.2502 BTU/lb-°F
Melting Point >= 532 °C>= 990 °FIncipient Melting
Solidus 605 °C1120 °F
Liquidus 632 °C1170 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 425 °C446 - 797 °FHot Working
Annealing Temperature 345 °C653 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.5 - 4.0 %2.5 - 4.0 %
Calcium, Ca <= 0.040 %<= 0.040 %
Copper, Cu <= 0.050 %<= 0.050 %
Iron, Fe <= 0.0050 %<= 0.0050 %
Magnesium, Mg 96 %96 %As Remainder
Manganese, Mn <= 0.080 %<= 0.080 %
Nickel, Ni <= 0.0050 %<= 0.0050 %
Silicon, Si <= 0.050 %<= 0.050 %
Zinc, Zn 0.70 - 1.6 %0.70 - 1.6 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polypropylene, Molded
Formosa Plastics Formolene® 5140H Compression Molding Polypropylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Low Density Polyethylene (LDPE), Molded

MMPE00 / 12459

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.