MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovako ISO 898 grade 10.9 42CrMnMo4-4,SAE 4140 (6115)) Steel, +QT
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: The steel grade variants are suitable for quenching and tempering to 8.8 or 10.9 properties. Required 90% martensite in the centre of the material is achieved up to diameter of each variant by oil quenching. The limiting factor for maximum size is the amount of the martensite in the core of the material. Therefore the same maximum diameters apply for 8.8 fasteners.

Information provided by Ovako

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 316 - 375
@Thickness 25.0 - 60.0 mm
Round bar
Tensile Strength >= 1040 MPa
@Thickness 25.0 - 60.0 mm
Round bar
Tensile Strength, Yield >= 940 MPa
@Thickness 25.0 - 60.0 mm
Round bar
Elongation at Break 9.0 %
@Thickness 25.0 - 60.0 mm
Round bar
Reduction of Area 48 %
@Thickness 25.0 - 60.0 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 27.0 J
@Thickness 25.0 - 60.0 mm,
Temperature -20.0 °C
Round bar, long
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 400 °CMS
 723 °CAC1
 827 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 - 0.45 %
Chromium, Cr 0.90 - 1.1 %
Iron, Fe 96.91 - 97.65 %As Balance
Manganese, Mn 0.75 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %
Phosphorus, P <= 0.020 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1040 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 8740 Steel, normalized 870°C (1600°F)
AISI 1141 Steel, cold drawn, high temperature, stress relieved, round
Overview of materials for Medium Carbon Steel
304 Stainless Steel

NOVAKO405 / 234704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.