System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LATI Latiohm 88/10-06 CNT PEEK
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Unreinforced
Material Notes:
Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.32
g/cc
0.0477
lb/in³
Linear Mold Shrinkage, Flow
0.0115
-
0.0155
cm/cm
0.0115
-
0.0155
in/in
Linear Mold Shrinkage, Transverse
0.012
-
0.0155
cm/cm
0.012
-
0.0155
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
90.0
MPa
13100
psi
Elongation at Break
35 %
35 %
Elongation at Yield
5.0 %
5.0 %
Tensile Modulus
4.00
GPa
580
ksi
Charpy Impact Unnotched
4.00
J/cm²
19.0
ft-lb/in²
Charpy Impact, Notched
0.500
J/cm²
2.38
ft-lb/in²
Electrical Properties
Metric
English
Comments
Volume Resistivity
15000
ohm-cm
15000
ohm-cm
Surface Resistance
3000
ohm
3000
ohm
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
200
°C
392
°F
Deflection Temperature at 1.8 MPa (264 psi)
160
°C
320
°F
Vicat Softening Point
>=
300
°C
@Load 5.00 kg
>=
572
°F
@Load 11.0 lb
Processing Properties
Metric
English
Comments
Melt Temperature
360
-
390
°C
680
-
734
°F
Mold Temperature
160
-
180
°C
320
-
356
°F
Drying Temperature
120
-
150
°C
@Time 10800 sec
248
-
302
°F
@Time 3.00 hour
Descriptive Properties
Electromagnetic reflection
88 dB
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Eurofoam Porocell POR 304 CM EPDM Foam
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK)
VICTREX™ PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced
VICTREX™ PEEK 150GL30 30% Glass Fiber Reinforced
PLATH9958 / 177654
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.