MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene NA270001 Low Density Polyethylene (LDPE), Wire/Cable Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Petrothene NA270001 is a high flow, low density polyethylene resin selected for use in the injection molding of caps, closures, other specialty applications or cast film. NA270001 is also used in wire & cable applications. NA270001 exhibit an excellent balance of toughness, softness, dimensional stability and processability. Applications: Carpet Backing, Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47ASTM D2240
Tensile Strength at Break 8.00 MPaASTM D638
Tensile Strength, Yield 11.0 MPaASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus, 1% Secant 186 MPaASTM D790
2% Secant Modulus 165 MPaASTM D790
 
Descriptive Properties
Processing MethodInjection Molding, Wire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PEQT8856 / 220490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.