MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Tecnoflon® FOR 421/U Fluorelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: TECNOFLON® FOR 421/U is a low viscosity cure incorporated fluoroelastomer copolymer. This grade is well suited for applications where superior flow, mold release, and excellent compression set are required. Tecnoflon® FOR 421/U can be compounded to meet the major fluoroelastomer specifications.

Some of the basic properties of Tecnoflon® FOR 421/U are:
- Very fast cure rate
- Very good scorch safety
- Superior mold flow
- Excellent mold release
- Lack of mold fouling
- Excellent compression set
- Good extrusion

TECNOFLON® FOR 421/U can be used for injection and transfer molding of O-rings, gaskets, and seals. The product can be mixed using typical fluoroelastomers compounding ingredients and mixing can be accomplished with two-roll mills or internal mixers.
The material can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting. Finished goods can be produced by a variety of rubber processing methods.

Applications: Belts/Belt Repair; Blending; Gaskets; Hose; Profiles; Seals; Sheet

Features: Copolymer; Fast Cure; Good Flow; Good Mold Release; Good Processability; Low Compression Set; Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 24
@Temperature 121 °C
24
@Temperature 250 °F
ML 1+10; ASTM D1646
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %
 
Descriptive Properties
AvailabilityEurope
 North America
ColorOff-White
FormsSlab
ProcessingCalendering; Compounding
 Extrusion; Injection Molding; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4503 / 280303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.