MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® IP 5565 ASTM D3568
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nordel® IP 5565 is an amorphous, high diene, EPDM grade designed for extruded applications requiring fast cure rates. It is ideally suited for continuously cured dense and sponge profiles. Molded applications will also benefit from the fast cure response, allowing shorter cycle times.

Information provided by manufacturer.

Key Words: 1155A18-04
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 63
@Temperature 100 °C
ML 1 + 4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 10.7 MPaVulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 301 %Vulcanizate, Press cured, TC95 +3min at 160°C
50% Modulus 0.00190 GPa
@Strain 50 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00400 GPa
@Strain 100 %
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00780 GPa
@Strain 200 %
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.0103 GPa
@Strain 300 %
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 26.0 kN/mDie C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 60 %
@Temperature 125 °C
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -41.0 °CTemperature Retraction, TR-10
 
Descriptive Properties
Formulation as Tested0.5TMTD
 1Stearic Acid
 1MBT
 1.5Sulfur
 100Nordel® IP 5565
 2ZnDBC
 5Zinc Oxide
 50Paraffinic Oil
 80N550 Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nordel® IP 4640 General Purpose Compound
Dow Nordel® IP 4640 Molded Brake Cup
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured
Dow Nordel® IP 4640 Dense Extruded Profile
Dow Nordel® IP 4570 Radiator/Heater Hose

PDVG46 / 34166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.