MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyPLASTY PolyPLEX PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes:

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.60 %0.60 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, H358/30 195 MPa28300 psiISO 2039-1
Hardness, Shore D 8181ISO 868, ISO 2039-2
Tensile Strength, Yield 73.0 MPa10600 psiISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Modulus of Elasticity 3.20 GPa464 ksiISO 527
Flexural Strength 130 MPa18900 psiISO 178
Fatigue Strength 10.0 MPa1450 psiflexure; ASTM D671
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2200 MPa319000 psi0.5 percent; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 3.7
@Frequency 50 Hz
3.7
@Frequency 50 Hz
IEC 60250
Dissipation Factor  0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 0.050
@Frequency 50 Hz
0.050
@Frequency 50 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359
Specific Heat Capacity 1.50 J/g-°C0.359 BTU/lb-°FIEC 1006
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52 612
Melting Point 110 °C230 °FISO 11357
Maximum Service Temperature, Air 80.0 °C176 °Flong term
 100 °C212 °Fshort term
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75
Vicat Softening Point 103 °C
@Load 5.10 kg
217 °F
@Load 11.2 lb
point B; ISO 306 VST/B/50
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0618 in
IEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)17ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Chemical Sumipex® MH Acrylic Resin, Heat Resistant
PolyPLASTY PolyPET PET
PolyPLASTY PolyPEEK PEEK
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

PPOLYPL927 / 197637

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.