MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Solvay THORNEL® T-300 Pan-Based Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: Description: THORNEL® T300 is a standard modulus fiber supplied with 1% UC.309 epoxy-compatible sizing. T300 1K, 6K and 12K products are offered in never-twisted form. T300 3K is offered in both twisted and never-twisted forms.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.76 g/cc
Specific Surface Area 0.45 m²/g
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 545000 psi
Elongation at Break 1.6 %
Tensile Modulus 231 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.600 µm/m-°C
Thermal Conductivity 8.00 W/m-K
 
Descriptive Properties
Carbon Assay92%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

PCYTED067 / 180369

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.