MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ AM Compound AF004XXAR1 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP THERMOCOMP AF004XXAR1 compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing 20% glass fiber for Large Format Additive Manufacturing (LFAM) applications. Added features of this grade include: Easy Processing, Low Warp and Good Print Surface quality, making them a good candidate material for a broad range of applications and tooling, including thermoforming and vacuum-forming.

Features: Low Warpage,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Moisture Absorption 0.0500 - 0.100 %0.0500 - 0.100 %Extrusion
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 21.0 MPa3050 psi5mm/min; ASTM D638 Modified
 63.0 MPa9140 psi5mm/min; ASTM D638 Modified
Elongation at Yield 1.0 %1.0 %5 mm/min; ZX ORIENTATION; ASTM D638 Modified
 1.8 %1.8 %5 mm/min; XZ ORIENTATION; ASTM D638 Modified
Tensile Modulus 0.00260 GPa0.377 ksi5 mm/min; ZX ORIENTATION; ASTM D638 Modified
 0.00510 GPa0.740 ksi5 mm/min; XZ ORIENTATION; ASTM D638 Modified
Flexural Strength 35.0 MPa5080 psi5 mm/min; ASTM D790 Modified
 91.0 MPa13200 psi5 mm/min; ASTM D790 Modified
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 103 °C
@Thickness 3.20 mm
217 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °FBed Temperature
Nozzle Temperature 210 - 250 °C410 - 482 °F
Zone 1 190 - 230 °C374 - 446 °FExtrusion
Zone 2 200 - 240 °C392 - 464 °FExtrusion
Zone 3 210 - 250 °C410 - 482 °FExtrusion
Zone 4 220 - 260 °C428 - 500 °FExtrusion
Melt Temperature 220 - 260 °C428 - 500 °FExtrusion
Drying Temperature 80.0 °C176 °FExtrusion
Dry Time 4.00 hour4.00 hourExtrusion
Hold Pressure <= 13.5 MPa<= 1960 psiExtruder Pressure
 
Descriptive Properties
Extruder L/D24

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82492 / 290439

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.