MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta RTB320Z Phenolic Linen Laminate Tube, NEMA LE
Categories: Polymer; Thermoset; Phenolic

Material Notes: RTB320Z is similar to RTB320X being composed of an extra-fine weave woven cotton fabric combined with a phenolic resin system. RTB320Z tubes have higher densities (minimum allowable specific gravity is 1.30) resulting in enhanced precise machining characteristics and are expected to give longer life in wear applications. Typical uses include retainers for ball-bearings. RTB320Z also complies with MIL-I-24768/13, Type FBE, ASTM D709 Type II Grade LE and Federal Specification WW-L-2887.

Information provided by Norplex-Micarta

Key Words: Linen, Phenolic, Micarta, NEMA LE, MIL-I-24768/13 Type PBE, ASTM D709 Type II Grade LE
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/cc0.750" X 1.000"; ASTM D792
Moisture Absorption 1.40 %0.750" X 1.000"; ASTM D570 Condition D1-24/23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 1050.750" X 1.000"; ASTM D785
Tensile Strength 11000 psi0.750" X 1.000"; ASTM D638 Condition A
Compressive Strength 33000 psi0.750" X 1.000"; ASTM D695 Condition A
Compressive Modulus 400 ksi0.750" X 1.000"; ASTM D695 Condition A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 200 V/mil0.750" X 1.000"; ASTM D149 Condition A
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 125 °C0.750" X 1.000"; UL Bulletin 746b
UL RTI, Mechanical with Impact 125 °C0.750" X 1.000"; UL Bulletin 746b
Flammability, UL94 HB0.750" X 1.000"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta RTB320S Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta RT342 Phenolic Cotton Laminate Tube, NEMA C
Norplex-Micarta RTB320X Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta RTB320H Phenolic Linen Laminate Tube, NEMA LE
Norplex-Micarta RT130X Epoxy Fiber Glass Laminate Tube, NEMA FR-4

PNORPM116 / 192855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.