MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical Lupox® DP1000DU PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Description: Injection Molding, PBT, General Purpose

CAS No. 30965-26-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.020 - 0.021 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 590 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 860 kg(f)/cm²
@Thickness 3.20 mm
2.8mm/min; ASTM D790
Flexural Modulus 25000 kg(f)/cm²
@Thickness 3.20 mm
2.8mm/min; ASTM D790
Izod Impact, Notched 3.30 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Strength 23.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 600 VSolution A; IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.30 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.30 mm
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C@ Break; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 174 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 140 °C
@Thickness >=0.710 mm
 140 °C
@Thickness >=1.50 mm
 140 °C
@Thickness >=3.30 mm
UL RTI, Mechanical with Impact 130 °C
@Thickness >=0.710 mm
 130 °C
@Thickness >=1.50 mm
 130 °C
@Thickness >=3.30 mm
UL RTI, Mechanical without Impact 140 °C
@Thickness >=0.710 mm
 140 °C
@Thickness >=1.50 mm
 140 °C
@Thickness >=3.30 mm
Flammability, UL94 HB
@Thickness >=0.710 mm
 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.30 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 245 - 255 °CInjection Molding
Middle Barrel Temperature 245 - 260 °CInjection Molding
Front Barrel Temperature 245 - 260 °CInjection Molding
Nozzle Temperature 250 - 265 °CInjection Molding
Mold Temperature 40.0 - 80.0 °CInjection Molding
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 60 1 (4659) PA66/6 Dry, 60% Glass Filled
LG Chemical Lupox® GP1000A PBT
Mitsubishi Chemical Advanced Materials Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet)
LG Chemical Lupox® GP1000S PBT
Cast Stainless Steel 440C, ASTM A276

PLAY285 / 148295

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.