Description: VESTODUR 1003-FR5 is an unreinforced, low-viscosity, quick setting semicrystalline thermoplastic compound for injection molding, based on polybutylene terephthalate (PBT). It has a white color. Test bars made of these compounds are rated V-0 according to UL94 by Underwriters Laboratories Inc., self-extinguishing and non-dripping. The compounds are especially suitable for parts which are subjected to high mechanical and thermal loads. Information provided by degussa. Evonik Industries is the successor company to Degussa. |