Notes: Monprene RG-65050 NAT is a specialty thermoplastic elastomer used in regulated consumer applications and complies with various US FDA and European regulations and directives for food contact. Monprene RG-65050 NAT is a low hardness, low density, RoHS compliant grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Food Contact Acceptable; Good Adhesion; Good Colorability; Good Melt Strength; Good Organoleptic Properties; Good Processability; Halogen Free; High Elongation; High Tensile Strength; Low Compression Set; Low Density; Low Hardness Uses: Closures; Consumer Applications; Cookware Handles; Cups; Film; Fluid Handling; Food Containers; Food Packaging; Food Service Applications; Gaskets; Kitchenware; Lids; Non-specific Food Applications; Overmolding; Toys; Toothbrush Handles; Toys; Tubing RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Preliminary data. Information provided by Teknor Apex |