MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Constellium Certal® SPC Forged Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in many types of applications. Typical applications include compression or injection moulds for plastics.

Information provided by manufacturer

Key Words: AA 7041 forged
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.82 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 140
@Thickness 450 - 700 mm
Temper T652
 150
@Thickness 400 - 450 mm
Temper T652
 155
@Thickness 325 - 400 mm
Temper T652
Tensile Strength >= 410 MPa
@Thickness 450 - 700 mm
Temper T652
 >= 430 MPa
@Thickness 400 - 450 mm
Temper T652
 >= 450 MPa
@Thickness 325 - 400 mm
Temper T652
 480 MPa
@Thickness 450 - 700 mm
Temper T652
 520 MPa
@Thickness 325 - 400 mm
Temper T652
 520 MPa
@Thickness 400 - 450 mm
Temper T652
Tensile Strength, Yield >= 340 MPa
@Strain 0.2 %,
Thickness 450 - 700 mm
Temper T652
 >= 350 MPa
@Strain 0.2 %,
Thickness 400 - 450 mm
Temper T652
 >= 370 MPa
@Strain 0.2 %,
Thickness 325 - 400 mm
Temper T652
 420 MPa
@Strain 0.2 %,
Thickness 450 - 700 mm
Typical Strength
 460 MPa
@Strain 0.2 %,
Thickness 325 - 400 mm
Typical Strength
 460 MPa
@Strain 0.2 %,
Thickness 400 - 450 mm
Typical Strength
Elongation at Break >= 3.0 %
@Thickness 325 - 400 mm
Temper T652
 >= 3.0 %
@Thickness 400 - 450 mm
Temper T652
 >= 3.0 %
@Thickness 450 - 700 mm
Temper T652
 7.0 %
@Thickness 400 - 450 mm
Typical Elongation
 7.0 %
@Thickness 450 - 700 mm
Typical Elongation
 8.0 %
@Thickness 325 - 400 mm
Typical Elongation
Modulus of Elasticity 73.0 GPacompression
Tensile Modulus 72.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.7 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.857 J/g-°C
Thermal Conductivity 153 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 89.08 - 92.35 %as balance
Chromium, Cr <= 0.040 %
Copper, Cu 0.40 - 0.90 %
Iron, Fe <= 0.25 %
Magnesium, Mg 1.5 - 2.3 %
Manganese, Mn <= 0.40 %
Silicon, Si <= 0.15 %
Titanium, Ti <= 0.060 %
Zinc, Zn 5.7 - 6.7 %
Zirconium, Zr 0.050 - 0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Constellium Certal® SPC Aluminum
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
Clinton Aluminum Alumold® 1-500 Forged
AISI 1008 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled

NCONS018 / 160281

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.