MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite PocoPyroGraph® Implant/Etch Grade Specialty Graphite  (discontinued **)
Categories: Carbon; Graphite

Material Notes: Shore hardness is 66. PocoPyroGraph® combines the superior characteristics of Poco semiconductor-grade graphites, with increased density and reduced porosity, to produce the material of choice for current and next generation implant and etch components.

Information provided by Poco Graphite, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.56 g/cc0.0564 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 53.4 MPa7750 psi
Compressive Yield Strength 97.9 MPa14200 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00200 ohm-cm0.00200 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.50 µm/m-°C
@Temperature 20.0 °C
4.17 µin/in-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99.9995 %99.9995 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating

EPOC11 / 5678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.