MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUMID GP2251BFH PA66+GF25%, Injection Molding
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Flame Retardant

Application: E&E Parts

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccASTM D792
Water Absorption 0.60 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 1350 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break 2.5 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Strength 206 MPa
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 90000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 7.50 kg-cm/cm
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D 257
Dielectric Constant 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Comparative Tracking Index 400 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°CASTM D696
Melting Point 260 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 130 °C
@Thickness 0.750 mm
UL 746B
UL RTI, Mechanical with Impact 100 °C
@Thickness 0.750 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.750 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.750 mm
 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 265 - 280 °C
Middle Barrel Temperature 270 - 290 °C
Front Barrel Temperature 270 - 290 °C
Nozzle Temperature 80.0 - 110 °C
Melt Temperature 270 - 290 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 - 100 °C
@Time 14400 - 18000 sec
Moisture Content <= 0.090 %
Back Pressure 0.981 - 2.94 MPaHydraulic
 9.81 - 29.4 MPaElectronic
Screw Speed 60 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
LG Chemical LUMID GN2251BF PA66+GF25%, Injection Molding
LG Chemical LUMID GP2301BFH PA66+GF30%, Injection Molding
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant

PLHCHEM9757 / 239273

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.