MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing enhanced surface appearance versus nylon 6/6 compounds. These materials are available in a broad range of reinforcement levels depending upon stiffness characteristics desired and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
Density 1.37 g/ccISO 1183
Filler Content 33 %Glass Fiber Reinforcement
Water Absorption 0.90 %@ 24 hrs; ASTM D570
 1.0 %24h/23C; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 172 MPaType I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 0.965 MPaISO 527-2
 165 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %ISO 527-2
Elongation at Yield 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8270 MPaASTM D638
 8300 MPaISO 527-2
Flexural Strength 1.52 MPaISO 178
 241 MPaASTM D790
Flexural Modulus 8270 MPaASTM D790
 8300 MPaISO 178
Izod Impact, Notched 110 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °CAnnealed; ISO 75-2/A
 206 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 48.9 - 93.3 °C
Drying Temperature 82.2 °C
Dry Time 4.00 hour
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceBlack
Automotive SpecificationsCHRYSLER MS-DB41 CPN2625
FeaturesGeneral Purpose
 Good Weather Resistance
 Heat Stabilized
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH0POL0961 / 145530

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.