MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek MTEK HK40 Cast UNS J94204 Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; Cast Stainless Steel

Material Notes: Increased strength for more highly stressed applications. Good resistance to oxidizing or reducing process flow.

Applications: Calcining tubes, pier caps, high temperature fixtures and hardware.

Information provided by MetalTek

Key Words: Cast UNS J94204; Cast Grade HK 40; Cast ASTM A297, A351, A608
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170
Tensile Strength, Ultimate >= 430 MPa
Tensile Strength, Yield >= 240 MPa
Elongation at Break >= 10 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1025 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.35 - 0.45 %
Chromium, Cr 23 - 27 %
Iron, Fe 47.3 - 57.65 %As Balance
Manganese, Mn <= 1.5 %
Nickel, Ni 19 - 22 %
Silicon, Si <= 1.75 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cast Stainless Steel HK40, ASTM A351M
Cast Stainless Steel HK, ASTM A297
HK40 CENTRIFUGALLY CAST 25Cr-20Ni-0.4C STEEL TUBES FOR USE IN REFORMER FURNACES (SCH 22-CF)
Cast Stainless Steel HX, ASTM A297
Cast Stainless Steel HK40, ACI

NMETEK093 / 18343

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.