MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carmel Olefins Ipethene® 670 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: IPETHENE® 670 is a low density polyethylene extrusion coating and lamination grade. This grade can be processed at high coating temperatures and coating speeds. It exhibits low neck-in and stable web edge, good adhesion to many substrates, excellent heat sealing properties, and low gel level.

APPLICATIONS

IPETHENE® 670 is mainly used for intermediate and light-weight high speed extrusion coating. It can be applied to various substrates such as paper, cardboard, aluminum foil, and flexible films like nylon, cellulose and polyester. The coated substrates can be used for packaging of foods, liquids and powders, medical devices, agricultural materials, chemicals and other industrial products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccISO 1183-A
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45ISO 868
Tensile Strength at Break 10.5 MPaISO 527-2
Tensile Strength, Yield 10.5 MPaISO 527-2
Elongation at Break 500 %ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 108 °CISO 11357
Vicat Softening Point 89.0 °C
@Load 1.02 kg
ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 4010 Low Density Polyethylene (LDPE)
A. Schulman CP851 High Flow, Injection Molding Grade
Bamberger Polymers Bapolene® 1072 Polyethylene, Injection Grade
Arkema LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate
Arkema LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PCARM013 / 79751

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.