MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® CP-22142 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-22142 is a high performance thermoplastic elastomer, available in natural and colors, designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-22142 is a translucent, medium hardness, low density, unfilled grade that is suitable for injection molding or extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Chemical Resistant; Good Colorability; Good Flexibility; Good Processability; Good Toughness; Low Density; Medium Hardness; Low Specific Gravity; Lubricated; Medium Flow; Resilient; Slip; Without Fillers

Uses: Consumer Applications; Flexible Grips; Gaskets; General Purpose; Grommets; Handles; Knobs; Luggage; O-rings; Overmolding; Plugs; Rubber Replacement; Safety Equipment; Seals; Sporting Goods

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  43
@Time 5.00 sec
43
@Time 0.00139 hour
Injection Molded; ASTM D2240
 45
@Time 1.00 sec
45
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 8.20 MPa1190 psi20 in/min, Flow; ASTM D412
 12.4 MPa1800 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  0.889 MPa
@Strain 100 %
129 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 1.72 MPa
@Strain 100 %
249 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
Elongation at Break 550 %550 %20 in/min, Flow; ASTM D412
 660 %660 %20 in/min, Across Flow; ASTM D412
Tear Strength 25.2 kN/m144 pli20 in/min, Across Flow; ASTM D624
Compression Set 14 %
@Temperature 22.8 °C,
Time 79200 sec
14 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 204 °C360 - 400 °FMelt, Injection
Rear Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Middle Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Front Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Nozzle Temperature 182 - 204 °C360 - 400 °FInjection
Zone 1 171 - 193 °C340 - 380 °FExtrusion
Zone 2 171 - 193 °C340 - 380 °FExtrusion
Zone 3 171 - 193 °C340 - 380 °FExtrusion
Zone 4 171 - 193 °C340 - 380 °FExtrusion
Zone 5 171 - 193 °C340 - 380 °FExtrusion
Die Temperature 171 - 193 °C340 - 380 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlue
 Colors Available
 Green
 Light Blue
 Natural Color
 Orange
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0812 / 237303

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.