Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This material provides a cost-effective alternative to carbon-filled PTFE. Special Properties: • Very good conductivity • Voltage dissipation on surface in less than 0.1s • Suitable for devices and machines subject to Directive 94/9/EC (ATEX 95) • Approved for use in the food industry (EU and FDA) Information provided by Murtfeldt Kunststoffe GmbH & Co. KG. |