MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® H 4320 AT POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Ultraform® H 4320 AT is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and low tendency to discolor. Typical applications include pipe and semi-finished parts for gear wheels, bearings and other mechanical elements.

Availability: North America

Features: Good Color Stability; Good Thermal Stability; High Molecular Weight

Use: Bearings; Gears; Piping

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Processing Method: Extrusion; Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption 0.25 %0.25 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.0 %1.0 %ISO 62
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/inISO 294-4
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-2
Elongation at Break 31 %31 %Nominal; ISO 527-2
Elongation at Yield 11 %11 %ISO 527-2
Tensile Modulus 2.40 GPa348 ksiISO 527-1
Izod Impact, Notched (ISO)  6.09 kJ/m²
@Temperature -30.0 °C
2.90 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 6.51 kJ/m²
@Temperature 22.8 °C
3.10 ft-lb/in²
@Temperature 73.0 °F
ISO 180
Charpy Impact Unnotched  25.2 J/cm²
@Temperature -30.0 °C
120 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 25.2 J/cm²
@Temperature 22.8 °C
120 ft-lb/in²
@Temperature 73.0 °F
ISO 179
Charpy Impact, Notched  0.546 J/cm²
@Temperature -30.0 °C
2.60 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.651 J/cm²
@Temperature 22.8 °C
3.10 ft-lb/in²
@Temperature 73.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 121 µm/m-°C67.0 µin/in-°FASTM E831
Melting Point 163 °C325 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 110 °C176 - 230 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 3.50 - 7.03 MPa508 - 1020 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2143 / 310836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.