MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sibur SKS-30 ARKM-27 2nd Group Oil-Filled Styrene-Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SBR 1712. For use in the tire industry for production of tire thread and other parts for tires, in the rubber technical industry for production of a wide assortment of rubber technical articles, and in the shoe industry for production of white an colored footwear.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 46 - 58
@Temperature 100 °C
ML 1-4
Ash <= 0.60 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22 - 25 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 21.5 MPa
Elongation at Break 550 - 570 %
 
Descriptive Properties
Loss During Drying<0.4%
Mass Share Adigol-20.8-1.5
Mass Share of A-Methyl Styrene22-25%
Mass Share of Oil26-29%
Mass Share of VS-10.3-0.7
Mass Share of VTS-1501-0.4
Spread Flow Batch Error<±7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIB105 / 67668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.