MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation at temperatures of 230°C. Other features are fast cycling and hot water moldability. This product is particularly suitable to air induction applications within downsized automotive engines such as air induction charge air cooling and exhaust gas recirculation.

Features: Fast Molding Cycle; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Hot Water Moldability; Laser Weldable; Low Moisture Absorption; Lubricated

Uses: Automotive Applications; Automotive Under the Hood; Metal Replacement

Injection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³Dry; ISO 1183
Filler Content 45 %45 %Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inDry
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDry; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 172 MPa24900 psiASTM D695
Shear Strength 75.8 MPa11000 psiASTM D732
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+14 ohm-cm5.00e+14 ohm-cmASTM D257
Dielectric Constant  3.4
@Frequency 1e+6 Hz
3.4
@Frequency 1e+6 Hz
ASTM D150
 4.3
@Frequency 60 Hz
4.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 1.60 mm
508 kV/in
@Thickness 0.0630 in
ASTM D149
Dissipation Factor  0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
ASTM D150
 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 600 V600 VUL 746
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min0.709 in/minUL 746
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °FDry; ISO 11357-3
 327 °C621 °FDry; DSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 318 - 324 °C604 - 615 °F
Front Barrel Temperature 327 - 332 °C621 - 630 °F
Melt Temperature 329 - 343 °C624 - 649 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content <= 0.045 %<= 0.045 %
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
 Mold Release
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormPellets
Processing TechniqueWater-Heated Mold Injection Molding

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y6947 / 176678

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.