MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive; Filled/Reinforced Thermoset

Material Notes: Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating flanges for salt spray corrosion protection when mounting an electrically conductive gasket between the surfaces.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.060 ohm
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 121 °C
 6.00 hour
@Temperature 65.0 °C
 168 hour
@Temperature 24.0 °C
Pot Life 480 min
@Temperature 24.0 °C
 480 min
@Temperature 23.9 °C
Shelf Life 9.00 Month@ 75°F
 9.00 Month
@Temperature 24.0 °C
 
Descriptive Properties
BinderEpoxy
ConsistencyMedium Fluid
FillerAg
Mix Ratio100:37
Spraying Viscosity, #2 Zahn Cup19 - 26 sec
Theoretical Yield50 ft2/lb1.5 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 1500 Polyester, Granular, Compression Molded
Haysite 14100 Polyester BMC, 15% Glass Reinforced
G-5 Fiberglass Melamine Laminate Sheet
G-3 Fiberglass Phenolic Laminate Sheet
G-11 Fiberglass Epoxy Laminate Sheet

PCHOME156 / 28378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.