Description: Release fabric. Ideally suited to flat or single curvature applications. Features & Benefits: - Medium porosity PTFE coated glass fabric
- Ideal for use on flat or single curvature moldings
- PTFE release coating ensures very easy release from the laminate without fear of contamination
- High performance material designed for use in extreme temperature and pressure processing conditions.
Information provided by Cytec, subsequently acquired by Solvay. |