MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EOS Aluminum AlF357 DMSL on EOS M 400
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Aluminum Alloy

Material Notes:

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.67 g/cc0.0965 lb/in³ISO 3369
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 330 MPa47900 psiheat treated state, Vertical
 340 MPa49300 psiheat treated state, Horizontal
 370 MPa53700 psiHorizontal
 390 MPa56600 psiVertical
Tensile Strength, Yield 250 MPa36300 psiVertical
 255 MPa37000 psiHorizontal
 265 MPa38400 psiheat treated state, Vertical
 270 MPa39200 psiheat treated state, Horizontal
Elongation at Break 5.0 %5.0 %Vertical
 8.0 %8.0 %Horizontal
 11.5 %11.5 %heat treated state, Horizontal
 11.5 %11.5 %heat treated state, Vertical
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°Fas built, Horizontal; ISO 22007-2
 140 W/m-K972 BTU-in/hr-ft²-°Fas built, Vertical; ISO 22007-2
 150 W/m-K1040 BTU-in/hr-ft²-°FT6, Horizontal; ISO 22007-2
 150 W/m-K1040 BTU-in/hr-ft²-°FT6, Vertical; ISO 22007-2
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 90.898 - 93.06 %90.898 - 93.06 %Balance
Beryllium, Be <= 0.0020 %<= 0.0020 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 0.10 %<= 0.10 %
Magnesium, Mg 0.40 - 0.70 %0.40 - 0.70 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Titanium, Ti 0.040 - 0.20 %0.040 - 0.20 %
Zinc, Zn <= 0.10 %<= 0.10 %
 
Descriptive Properties
Volume rate17 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS921 / 280581

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.