MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Washed 757 High Purity High-Index Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These fibers can be classified into the following general categories:

  • High-Index Fibers
  • High-Temperature Fibers
  • Large-Diameter Fibers
  • Milled Fibers

Fiber index is a measurement which determines the amount of fiberized material in the actual fiber. During fiber manufacturing, shot or unfiberized materail is produced as a natural product of the fiberization process. Unifrax has the ability to reduce the amount of shot in a fiber by controlling the furnacing process or by washing out the unfiberized material. Fiberfrax High-Index have proven to be a good reinforcement material for use in automotive break lining and other friction material. These high-index fibers provide a variety of desirable properties such as:

  • Frictional stability
  • High-temperature frictional performance
  • Fade resistance
  • Flexural reinforcement

Fiberfrax High-Index fibers can also be used as a mechanical thixotrope in coatings applications offering reinforcement and fire resistance as additional benefits. These fibers offer the following unique properties

  • Excellent high-temperature stability
  • Good strength and high modulus
  • Low coefficient of thermal expansion
  • Superior chemical resistance
  • Very low moisture absorption

The thixotropic properties of Fiberfrax High-Index Fibers in conjunction with the mechanical and physical properties they have to offer make them an excellent candidate for use in:

  • Mastics
  • Adhesives
  • Thick Film Coatings
  • Fire Protective Materials
  • Caulks, Putties, and Sealants

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.73 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1175 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 - 52 %
NaO2 <= 0.50 %
SiO2 48 - 53 %
 
Descriptive Properties
Average Fiber Diameter (microns)1-2.5
ColorWhite
Fiber Index (%)80
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Washed 707 High Purity High-Index Fiber
Unifrax Fiberfrax® Washed 657 High Purity High-Index Fiber
Unifrax Fiberfrax® HSA-K Kaolin High-Index Fiber
Unifrax Fiberfrax® HSA-HP High Purity High-Index Fiber
Unifrax Fiberfrax® HS95C High Purity High-Index Fiber

CUNIF066 / 97838

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.