MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell CirculenRecover HD5603 Ivory Plus HDPE
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: CirculenRecover HD5603 Ivory Plus is a circular high density polyethylene grade supplied in pellet form for blow molding applications. This grade is available in ivory color and characterized by its low residual odor, easy processability and colorability.

Sustainability: According with the requirements of Standard ISO 14021:2016, CirculenRecover HD5603 Ivory Plus contains at least 98% of recycled material that is fully based on Post-Consumer Waste (PCW) from pre-sorted municipal plastic waste. Filtration level is 150 µm. Volatiles according to ASTM D6980 @ 120 °C are < 0.1%. Based on CIELab values, the color indication is close to RAL 9018.

This product is not intended for highly regulated applications including food contact, potable water contact, medical and pharmaceutical applications.

Availability: Europe

Application: Bottles For Consumer Goods; Bottles for Industrial Use; General Sheet Extrusion

Market: Consumer Products; Industrial Packaging; Rigid Packaging

Processing Method: Extrusion Blow Molding

Attribute: Antioxidant; General Purpose; High Rigidity

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.956 g/cc0.0345 lb/in³ISO 1183-1
Melt Flow  0.300 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.300 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 1.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.50 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
Ash <= 2.00 %
@Temperature 600 °C
<= 2.00 %
@Temperature 1110 °F
ISO 3451-1
 
Mechanical PropertiesMetricEnglishComments
PENT 8.00 hour
@Pressure 6.00 MPa,
Temperature 50.0 °C
8.00 hour
@Pressure 870 psi,
Temperature 122 °F
FNCT, 2% Arkopal N100; ISO 16770
Tensile Strength, Yield 24.0 MPa3480 psiISO 527-1, -2
Elongation at Yield 9.00 %9.00 %ISO 527-1, -2
Tensile Modulus 1.20 GPa174 ksiISO 527-1, -2
Charpy Impact, Notched 0.250 J/cm²
@Temperature -30.0 °C
1.19 ft-lb/in²
@Temperature -22.0 °F
Type 1, Edgewise, Notch A; ISO 179
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9050 / 323978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.