MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials Starex® EG-7000 ABS/PET, Unreinforced
Categories: Polymer; Thermoplastic; ABS Polymer; ABS/Polyester Alloy; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 35 g/10 min
@Load 10.0 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ASTM D785
Tensile Strength, Yield 390 kg(f)/cm²50 mm/min; ASTM D638
Elongation at Break 40 %50 mm/min; ASTM D638
Flexural Strength 55.9 MPa2.8 mm/min; ASTM D790
Flexural Modulus 20000 kg(f)/cm²2.8 mm/min; ASTM D790
Izod Impact, Notched 21.0 kg-cm/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 88.0 °CB/50; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm
 
Optical PropertiesOriginal ValueComments
Yellow Index 20 %
@Thickness 3.20 mm
ASTM D1925

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® GC-0770 H ABS/PET, Unreinforced Recycled
Lotte Advanced Materials Starex® GC-0730 ABS/PET
Lotte Advanced Materials Starex® EG-7030 ABS/PET
Trinseo EMERGE™ 5302 Acrylonitrile Butadiene Styrene (ABS)
Lotte Advanced Materials Starex® SR-7300 ABS/PET, Unreinforced

PSAMSU729 / 146546

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.