MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sinvicomp SSZ6309 KD11 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Sinvicomp SSZ6309 KD11 is a wire & cable polyvinylchloride compound available in pellet form. It provides good performance for jacketing of cables.

Availability: Asia Pacific

Wire Types (BS 6746): TM1; TM2

RoHS Compliant:RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
Carbon Black Loading 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78ASTM D2240
Tensile Strength, Yield 2030 psiIEC 60811-1-1
 2130 psi
@Treatment Temp. 80.0 °C,
Time 605000 sec
Change after Aging in Air Oven; IEC 811-1-2
 2330 psi
@Treatment Temp. 70.0 °C,
Time 14400 sec
Change in IRM 902 Oil; IEC 60811-2-1
Elongation at Break 250 %IEC 60811-1-1
 275 %
@Treatment Temp. 80.0 °C,
Time 605000 sec
Change after Aging in Air Oven; IEC 811-1-2
 313 %
@Treatment Temp. 70.0 °C,
Time 14400 sec
Change in IRM 902 Oil; IEC 60811-2-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmBS 2782
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -18.4 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 170 °CCompression zone
 170 - 175 °CMixing zone
Feed Temperature 150 °C
Nozzle Temperature 175 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel
Carpenter No. 610® High Carbon, High Chrome Tool Steel (Air-Wear) (AISI D2)

PTEKNQ1578 / 238069

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.