MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inovyn 382NG Polyvinyl Chloride Homopolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: Polyvinyl chloride made by microsuspension polymerization. Uses: Spread coating - flooring top coat. Attributes: High filler acceptance; Matte appearance in flooring top coat; Good viscosity stability on storage.

Information provided by SolVin.

SolVin is a predecessor company to Inovyn.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content <= 0.30 g/lISO 1269
Particle Size <= 125 µm<0.2 g/kg retained on 125 micron sieve; ISO 787-18
Viscosity Measurement 82K value; ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 374MB Polyvinyl Chloride Medium Viscosity Paste
Inovyn 370HD Polyvinyl Chloride High Viscosity Paste
Inovyn 372NF Polyvinyl Chloride Low Viscosity Paste
Inovyn 367NF Polyvinyl Chloride Low Viscosity Paste
Inovyn 550GA Copolymer of Vinyl Chloride and Vinyl Acetate

PSOLVI39f / 146803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.