MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M AC-251 Black Class B-1 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate aircraft canopies and windshields. 3M AC-251 Black Class B Sealants contain no solvents and do not craze. The sealants quickly cure and exhibit excellent adhesion and resistance to UV and weather exposure. 3M AC-251 Black Class B Sealants have a thixotropic, non-sag consistency. They can be readily applied with a spatula or extrusion gun on vertical surfaces.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/cccured 14 days @ 50% RH; AMS-S-8802
Volatiles 2.0 %
Brookfield Viscosity 900000 - 1.60e+6 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55cured 14 days @ 50% RH; AMS-S-8802
Tensile Strength at Break 2.41 MPa
@Time 1.21e+6 sec
Standard Cure
 2.14 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
Elongation at Break 370 %
@Time 1.21e+6 sec
Standard Cure
 300 %
@Treatment Temp. 121 °C,
Time 605000 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CAMS-S-8802, cured 14 days @ 50% RH
 182 °CAMS-S-8802, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °CAMS-S-8802, cured 14 days @ 50% RH
 
Processing PropertiesOriginal ValueComments
Cure Time 7.00 hour
Tack-Free Time 5.00 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
AppearanceBlack
 BlackBase
 BlackAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M AC-251 Black Class B-2 Aerospace Sealant
3M AC-251 Black Class B-1/2 Aerospace Sealant

PMM35415 / 170162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.