MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses strong dimensional stability and chemical resistance. In addition, the effect of water absorption, which is a traditional weakness of polyamides, has been reduced to a minimum.

Applications:

  • Connectors
  • Jacks
  • Switches
  • Power supply terminals
  • Various cases

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D792
Filler Content 30 %
Water Absorption 0.3 %
@Thickness 2.00 mm
24 hours in 23°C water; ASTM D570
 3.0 %
@Thickness 2.00 mm
24 hours in 100°C water; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
Vertical Direction; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 110ASTM D785
Tensile Strength at Break 170 MPaASTM D638
Elongation at Break 3.0 %Measured between the chucks; ASTM D638
Flexural Strength 260 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Izod Impact, Notched 80.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 28.0 kV/mmASTM D149
Dissipation Factor 0.018
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
Vertical Direction; ASTM D696
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 310 °C
Deflection Temperature at 1.8 MPa (264 psi) 300 °CASTM D648
Glass Transition Temp, Tg 85.0 °C
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Feed Temperature 50.0 - 90.0 °CHopper Bottom for Electronic and Electric Standard Molding
 50.0 - 90.0 °CHopper Bottom Temp for Mechanical and Structural Standard Molding
Nozzle Temperature 315 - 335 °CNH Cylinder Temp for Electronic and Electric Standard Molding
 325 - 340 °CNH Cylinder Temp for Mechanical and Structural Standard Molding
Zone 1 300 - 325 °CC1 Cylinder Temp for Electronic and Electric Standard Molding
 315 - 330 °CC1 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 2 315 - 335 °CC2 Cylinder Temp for Electronic and Electric Standard Molding
 320 - 335 °CC2 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 3 320 - 335 °CC3 Cylinder Temp for Electronic and Electric Standard Molding
 325 - 340 °CC3 Cylinder Temp for Mechanical and Structural Standard Molding
Mold Temperature 90.0 - 140 °Cfor Electronic and Electric Standard Molding
 90.0 - 140 °Cfor Mechanical and Structural Standard Molding
Screw Speed 150 rpmfor Mechanical and Structural Standard Molding
 150 rpmfor Electronic and Electric Standard Molding
 
Descriptive Properties
Injection PressureMediumElectronic and Electric Standard Molding
 MediumMechanical and Structural Standard Molding
Injection SpeedMediumElectronic and Electric Standard Molding
 MediumMechanical and Structural Standard Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND)
Mitsui Arlen™ CH245NK 45% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
Mitsui Arlen™ C230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
Mitsui Arlen™ C240 40% Glass Fiber-Reinforced Modified Nylon 6T (DAM)

PMIT002 / 53178

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.