MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Conformable with: Q/DYS 003-2007

Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coefficient of friction, enabling thermoplastic processing methods. DS608 are high molecular weight resins of low melt index, with low extrusion temperature, high extrusion speed which is 5 ~ 8 times of ordinary FEP resin. It is soft, anti-burst, and has good toughness.

Main Applications:

Mainly for aviation and aerospace industry, the MTR transport vehicles, automatic switching equipment, well test equipment, flame alarm systems, high-rise buildings, fire regional wires, cables, computers, communication networks, electrical fields, particularly applicable for high-speed extrusion small-caliber wire insulation material. It is more economical when used where no high stress cracking resistance is required.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.14 - 2.17 g/cc
Volatiles <= 0.10 %
Melt Flow 12.1 - 16 g/10 minD
 16.1 - 20 g/10 minA
 20.1 - 24 g/10 minB
 24.1 - 28 g/10 minC
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 16.0 MPa
 >= 18.0 MPa
 >= 20.0 MPa
 >= 20.0 MPa
Elongation at Break >= 250 %
 >= 270 %
 >= 300 %
 >= 300 %
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant <= 2.15
@Frequency 1e+6 Hz
Dissipation Factor <= 0.00070
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 - 275 °C
 
Descriptive Properties
AppearanceTranslucent particles, without impurities such as metal debris and sand, containing visible black particles less than 2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® NP-101 FEP
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
ScanTube FEP Tubing
Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer
Shandong Dongyue Shenzhou New Material Co DS602 Perfluorinated Ethylene-Propylene Copolymer

PSHEN038 / 104093

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.