MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® A 2546 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Anionic polyacrylate dispersion. Binder for the formulation of water-reducible, two-component polyurethane coatings and sealers for mineral substrates and reactive resins (EP, PUR).

Properties / Applications: On account of its outstanding mechanical and chemical resistance, the product is particularly suitable for the formulation of sealers for mineral substrates and reactive resins (EP, PUR), in particular when good hot tire resistance is required. The product can also be combined with other water-reducible binders. On account of the many potential co-reactants, compatibility testing should always be carried out.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccDIN EN ISO 2811-2
Volatiles 58 - 62 %1g/1h/125 °C/convection oven; DIN EN ISO 3251
pH 7.0 - 9.01:3 in demineralized water; DIN ISO 976
Viscosity <= 200 cPD= approx. 45 s-1; DIN EN ISO 3219/A.3
 
Descriptive Properties
Content4.8%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0155 / 201938

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.