Telcar TL-2657J BLK is a general purpose thermoplastic elastomer designed for the industrial and transportation markets, including weatherstripping and wind skirts. It is a high hardness, high density, UV stable grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; High Density; High Hardness; High Specific Gravity; Light Stabilized; Low Flow; Sunlight Resistant; UV Resistant Uses: General Purpose; Grommets; Industrial Applications; Rubber Replacement; Weatherstripping RoHS Compliant:RoHS Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |