MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.

Data provided by Composite Technologies (CTC).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 12 g/10 min12 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiISO 527-1/2
Flexural Modulus 0.705 GPa102 ksi0.05 in/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²partial break, Low Temp; ISO 180/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 216 °C360 - 420 °F
Middle Barrel Temperature 193 - 227 °C380 - 440 °F
Front Barrel Temperature 204 - 216 °C400 - 420 °F
Nozzle Temperature 204 - 216 °C400 - 420 °F
Melt Temperature 204 - 227 °C400 - 440 °F
Mold Temperature 26.7 - 60.0 °C80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa4000 - 5000 psi
 
Descriptive Properties
Boost Pressure (psi)500-1500
ColorGeneral Purpose Black
Hold Pressure50 - 75% of Boost
Screw SpeedMedium to Fast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Dow Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin
CTC X-PRO TF 1020 GP Polypropylene Homopolymer, 20% Talc Filled

PCTC959 / 104732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.