MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sharadaa Ceramics VELECRETE RC 108 Rodding Castables
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in compliance with international standards.

Bond: Ultrafine

Aggregate: Andalusite + Cal.Bauxite

Type of Setting: Hydraulic

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.80 g/ccAfter Drying at 110°C
Grain Size <= 10000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0200 GPa
@Temperature 1000 °C
Cold
 0.0240 GPa
@Temperature 110 °C
Cold
 0.0240 GPa
@Temperature 1400 °C
Cold
 0.0250 GPa
@Temperature 1100 °C
Hot
Compressive Strength 1020 kg(f)/cm²
@Temperature 1000 °C
Cold Crushing
 1220 kg(f)/cm²
@Temperature 110 °C
Cold Crushing
 1220 kg(f)/cm²
@Temperature 1400 °C
Cold Crushing
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.09 W/m-K
@Temperature 600 °C
Hot Face
Maximum Service Temperature, Air 1700 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 68 %
Fe2O3 1.2 %
 
Descriptive Properties
Permanent Linear Change1at 1700°C
Resistance to AccretionExcellent
Thermal Expansion1at 1100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSHARA044 / 130207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.