MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zeon Specialty Materials ZEONEX® RS420 Cyclo Olefin Polymer  (discontinued **)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Ultra-low dielectric loss and dielectric constant for antenna substrate; high impact strength

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Water Absorption <= 0.010 %ASTM D570
Melt Flow 8.0 g/10 min
@Load 2.18 kg,
Temperature 280 °C
JIS 6719
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaISO 527
Elongation at Break 135 %ISO 527
Tensile Modulus 1700 MPaISO 527
Flexural Modulus 1600 MPaISO 178
Izod Impact, Notched 510 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.2
@Frequency 1e+9 Hz
ASTM D150
Dissipation Factor <= 0.0010
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CASTM E831
Glass Transition Temp, Tg 134 °CJIS K7121
 
Descriptive Properties
Colorwhite
Featuresgood moldability
Primary MarketAntenna carrier
Processing MethodExtrusion
REACHYes
RoHSYes
Usescable insulation layer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zeon Specialty Materials ZEONEX® 480R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® RS420-LDS Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® 790R Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® 480 Cyclo Olefin Polymer
Zeon Specialty Materials ZEONEX® K26R Cyclo Olefin Polymer

PZEONC81 / 73140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.