MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastobond 19412 Copolyester, Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastobond 19412 may be dried in a desicated drying system at 150 F. It offers excellent organoleptic and gas-barrier properties. Eastobond 19412 has low postextrusion crystallinity and a low softening point, enabling heat-seal bonds to be achieved over a temperature range of 95°C to 205°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccCrystalline Density; ASTM D1505
Bulk Density 0.715 g/cc0.0258 lb/in³ASTM D1895
Density 1.31 g/cc0.0473 lb/in³Film Density; ASTM D1505
Melt Density 1.20 g/cc
@Temperature 285 °C
0.0434 lb/in³
@Temperature 545 °F
ASTM D1238
Water Vapor Transmission 39.0 g/m²/day2.51 g/100 in²/dayASTM F372
Oxygen Transmission 3.10 cc-mm/m²-24hr-atm7.87 cc-mil/100 in²-24hr-atmASTM D3985
Carbon Dioxide Transmission 16.7 cc-mm/m²-24hr-atm42.4 cc-mil/100 in²-24hr-atmASTM D1434
Viscosity Measurement 0.650.65Inherent, Film; EMN-A-AC-G-V-1
 0.740.74Inherent; EMN-A-AC-G-V-1
Thickness 50.0 microns1.97 milASTM D374
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiASTM D638
Elongation at Break <= 5.0 %<= 5.0 %ASTM D638
Tensile Modulus 2.20 GPa319 ksiASTM D882
Elmendorf Tear Strength, MD 0.600 g/micron15.2 g/milASTM D1922
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.15 J/g-°C0.275 BTU/lb-°FDSC
 1.60 J/g-°C0.382 BTU/lb-°FDSC
 1.80 J/g-°C
@Temperature 125 °C
0.430 BTU/lb-°F
@Temperature 257 °F
DSC
 2.00 J/g-°C
@Temperature 200 °C
0.478 BTU/lb-°F
@Temperature 392 °F
DSC
 2.15 J/g-°C
@Temperature 290 °C
0.514 BTU/lb-°F
@Temperature 554 °F
DSC
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FASTM C177
Glass Transition Temp, Tg 51.0 °C124 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Haze <= 0.50 %<= 0.50 %ASTM D1003
Gloss 95 %95 %at 45°; ASTM D2457
Transmission, Visible 90 %90 %Regular Transmittance; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PE9067 / 35123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.