MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are designed to meet the challenging demands of the automotive, aerospace and chemical processing industries, requiring low temperature sealing in chemically aggressive environments. LTFE 6400Z offer a unique low temperature sealing capability of TR10 = -40°C as well as broad chemical resistance.

    Features and Benefits:
  • TR10 = -40°C which means true dynamic sealing capability at low temperatures
  • Very good chemical resistance against most chemicals such as acids, bases, fuels, oils, coolants, and alcohols
  • Processes comparably to other peroxide-cured fluoroelastomers
  • Good compression set resistance with low/no post-cure

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.86 g/cc
Mooney Viscosity 100
@Temperature 121 °C
ML 1+ 10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68Press Cure 10 Minutes @ 177°C
 70Post Cure 16 Hours @ 230°C
Tensile Strength at Break 11.9 MPaPress Cure 10 Minutes @ 177°C
 13.3 MPaPost Cure 16 Hours @ 230°C
Elongation at Break 175 %Post Cure 16 Hours @ 230°C
 180 %Press Cure 10 Minutes @ 177°C
100% Modulus 0.00610 GPa
@Strain 100 %
Post Cure 16 Hours @ 230°C
 0.00610 GPa
@Strain 100 %
Press Cure 10 Minutes @ 177°C
Compression Set 15 %
@Treatment Temp. 150 °C,
Time 252000 sec
Method B, -214 O-rings, Aged 70 Hours; ASTM D395
 26 %
@Treatment Temp. 200 °C,
Time 252000 sec
Method B, -214 O-rings, Aged 70 Hours; ASTM D395
 32 %
@Treatment Temp. 200 °C,
Time 605000 sec
Method B, -214 O-rings, Aged 168 Hours; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -40.0 °CTR10
Brittleness Temperature -60.0 °C
Glass Transition Temp, Tg -40.0 °C
Transformation Temperature -40.0 °CTR10; ASTM D1329
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 25 %translucent, but thickness not quantified
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 67.1 %
 
Descriptive Properties
ColorTranslucent, Clear-Amber
FormSlab
MH, Maximum Toque14.0 Inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque4.0 Inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t2, Time to 2 Inch-lb Rise from Minimum0.5 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t'50, Time to 50% Cure0.7 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t'90, Time to 90% Cure2.3 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® N2644 Z9 POM + PUR
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
Evonik VESTAGON® B 1400 PUR System
Avient OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, PUR
BASF Ultraform® N2650 Z6 POM + PUR

PDYL9962 / 129980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.