MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP7033L1 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like boxes, buckets, containers and crates and other consumer and industrial applications.

Availability: Africa & Middle East and Europe

Features:

  • Low Flow
Uses:
  • Consumer Applications
  • Containers
  • Industrial Applications
  • Tool/Tote Box
Processing Method: Injection Molding, Sheet Extrusion and Thermoforming

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ISO 868
Tensile Strength, Yield 3630 psiISO 527-2/50
Elongation at Yield 9.0 %ISO 527-2/50
Tensile Modulus 160000 psiISO527-2/1
Flexural Modulus 145000 psiSecant; ISO 178
Izod Impact, Notched (ISO) 3.60 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 1.90 ft-lb/in²
@Temperature -20.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 0.000 °C
ISO 179/1eA
 5.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 322 °FISO 3146
Crystallization Temperature 235 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 169 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 117 °FISO 75-2/A
Vicat Softening Point 295 °FISO 306/A50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP7011L1 Polypropylene Impact Copolymer
ExxonMobil PP4031E2 Polypropylene Impact Copolymer
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
ExxonMobil PP7032E2 Impact Copolymer

PEX99426 / 175662

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.